Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMT 402 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with very high stiffness, high heat ageing resistance and detergent resistance designed for electrical applications such as washing ma.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMU 202 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and low emissions for automotive HVAC and under-the-hood applications.Availability: Africa & Middl.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMU 208 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin, black colored, with high stiffness and release agent for automotive HVAC and under-the-hood applications.Availability: Africa & Middl.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ HMU 216 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by high stiffness and designed for automotive exterior applications in which good surface finish and good UV resistance .. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
ISO 179 |
ExxonMobil Exxtral™ HMU 405 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high heat ageing resistance, high transparency, low color and low discoloration for contact with hot water, hot air and detergent.. |
|||
Charpy Impact, Notched | 0.294 J/cm² @Temperature 22.8 °C |
1.40 ft-lb/in² @Temperature 73.0 °F |
ISO 179/1eA |
ExxonMobil PP1014H1 Polypropylene Homopolymer Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE.. |
|||
Charpy Impact, Notched | 0.294 J/cm² | 1.40 ft-lb/in² | ISO 179/1eA |
ExxonMobil PP1064L1 Polypropylene Homopolymer Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other .. |
|||
Charpy Impact, Notched | 0.294 J/cm² | 1.40 ft-lb/in² | ISO 179 |
ExxonMobil PPT0170F Polypropylene Homopolymer Product Description: PPT0170F is an unstabilized homo polymer granular resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation prov.. |
|||
Charpy Impact, Notched | 0.294 J/cm² | 1.40 ft-lb/in² | ISO 179/1eA |
ExxonMobil PP1364E2 Polypropylene Homopolymer Product Description: A medium melt flow homopolymer resin suitable for masterbatch carrier and other compounding applications and for the molding of garden furniture, caps and other consumer produc.. |