Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.210 - 1.00 J/cm² @Temperature -30.0 - 30.0 °C |
0.999 - 4.76 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.582 J/cm² Grade Count:31 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Charpy Impact, Notched | 0.210 - 7.50 J/cm² | 0.999 - 35.7 ft-lb/in² | Average value: 0.984 J/cm² Grade Count:155 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1230 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1230 L is a 30% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ASTM D256 |
Plenco 4759 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ASTM D256 |
Plenco 7300 Phenolic, Nodular, Injection Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ASTM D256 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | J/cm; ASTM D256 |
Plenco Valite 759 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4759. Data provided by Plenco.VALITE 759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and p.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 0.210 J/cm² @Temperature 23.0 °C |
0.999 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Charpy Impact, Notched | 0.210 J/cm² @Temperature 23.0 °C |
0.999 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.210 J/cm² | 0.999 ft-lb/in² | |
Biomer P209 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Charpy Impact, Notched | 0.210 - 5.40 J/cm² | 0.999 - 25.7 ft-lb/in² | Average value: 1.36 J/cm² Grade Count:26 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |