Polymer Property : Charpy Impact, Notched = 6.70 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 6.70 J/cm²
31.9 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific)
Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color..
Charpy Impact, Notched 6.70 J/cm²
31.9 ft-lb/in²
ISO Data
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Charpy Impact, Notched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eA
FKuR Kunststoff Terralene® LL 1101 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..
Charpy Impact, Notched 6.70 J/cm²
31.9 ft-lb/in²
ISO 179
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP
SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit
Charpy Impact, Notched 6.70 J/cm²
31.9 ft-lb/in²
ISO 179
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic..
Charpy Impact, Notched 6.70 J/cm²
31.9 ft-lb/in²
ISO 179
Teijin Panlite® LV-2225L Standard (mold release/ice color grade) Polycarbonate Resin
Flame retardant and mold release grade with high fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for thin wall injection moldings.Applications:Electric, ele..