Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | Partial Break |
Eastman Eastar DN007 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | ISO 179 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | ISO Data |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Charpy Impact, Notched | 6.10 J/cm² | 29.0 ft-lb/in² | ISO Data |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |