Polymer Property : Charpy Impact, Notched = 14.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched >= 14.0 J/cm²
>= 66.6 ft-lb/in²
ISO 179
Murtfeldt Material ”S”® 1000 Black Antistatic Polyethylene, Conductive
Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio..
Charpy Impact, Notched >= 14.0 J/cm²
>= 66.6 ft-lb/in²
ISO 179
Murtfeldt Original Material ”S”® plus + TLS Polyethylene
Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i..
Charpy Impact, Notched 14.0 J/cm²
66.6 ft-lb/in²
Sibur ABS 0809M Molding Grade ABS Plastic
Shock resistant with high thermal resistance for production of structural and decorative parts and articles of technical purpose.
Charpy Impact, Notched 14.0 J/cm²

@Temperature -20.0 °C
66.6 ft-lb/in²

@Temperature -4.00 °F
After conditioning at 23°C/50%RH; ISO 179/Af
Arkema Group Orgalloy® R 60 ES Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
Charpy Impact, Notched 14.0 J/cm²
66.6 ft-lb/in²
Longitudinal direction; ISO 179/2fn
Azdel Plus U400-B01N 41.5% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U400-B01N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. Thi..