Polymer Property : Charpy Impact, Notched = 1.06 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.06 - 1.30 J/cm²

@Temperature -30.0 - 30.0 °C
5.04 - 6.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 1.14 J/cm² Grade Count:3
Overview of materials for Nylon 12, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact, Notched 1.06 J/cm²

@Temperature 23.0 °C
5.04 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 1.06 J/cm²
5.04 ft-lb/in²
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Dry)
Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas..
Charpy Impact, Notched 1.06 J/cm²

@Temperature -30.0 °C
5.04 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Charpy Impact, Notched 1.06 J/cm²

@Temperature -30.0 °C
5.04 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BECN TL Nylon 11, Sheathing Grade (Conditioned)
Designation ISO 1874-PA11,KHL,12-010Rigid grade for sheathing of wires and cables. Available color: natural. Light and heat stabilized.High abrasion resistance. Well adapted melt viscosity. Ability ..
Charpy Impact, Notched 1.06 J/cm²

@Temperature -30.0 °C
5.04 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned)
Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d..
Charpy Impact, Notched 1.06 J/cm²
5.04 ft-lb/in²
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Dry)
Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo..
Charpy Impact, Notched 1.06 J/cm²

@Temperature -30.0 °C
5.04 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..