Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.930 J/cm² | 4.43 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**) Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15.. |
|||
Charpy Impact, Notched | 0.930 J/cm² | 4.43 ft-lb/in² | ISO 179/1eA |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Charpy Impact, Notched | 0.930 J/cm² | 4.43 ft-lb/in² | ISO 179 |
Solvay Specialty Polymers Amodel® DW-1140 Polyphthalamide (PPA), 40% Glass Fiber Amodel® DW-1140 is a 40% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o.. |
|||
Charpy Impact, Notched | 0.930 J/cm² | 4.43 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Charpy Impact, Notched | 0.930 J/cm² | 4.43 ft-lb/in² | EN ISO 179/1eA |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |
|||
Charpy Impact, Notched | 0.930 J/cm² @Temperature 23.0 °C |
4.43 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |