Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.330 J/cm² @Temperature -30.0 °C |
1.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.330 J/cm² | 1.57 ft-lb/in² | ISO 179/1eA |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature -30.0 °C |
1.57 ft-lb/in² @Temperature -22.0 °F |
|
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Charpy Impact, Notched | 0.330 - 1.22 J/cm² @Temperature -30.0 - -30.0 °C |
1.57 - 5.81 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.726 J/cm² Grade Count:10 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature 23.0 °C |
1.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature 23.0 °C |
1.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature -20.0 °C |
1.57 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2300-NC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Charpy Impact, Notched | 0.330 J/cm² | 1.57 ft-lb/in² | |
LATI Latishield 66-10A PA66, Steel Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Charpy Impact, Notched | 0.330 J/cm² | 1.57 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Charpy Impact, Notched | 0.330 J/cm² | 1.57 ft-lb/in² | ISO 179-1 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature -30.0 °C |
1.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature 23.0 °C |
1.57 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature 23.0 °C |
1.57 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Charpy Impact, Notched | 0.330 J/cm² @Temperature -30.0 °C |
1.57 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength.. |
|||
Charpy Impact, Notched | 0.330 J/cm² | 1.57 ft-lb/in² | ASTM D256 |
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Charpy Impact, Notched | 0.330 - 0.740 J/cm² @Temperature -30.0 - -30.0 °C |
1.57 - 3.52 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.497 J/cm² Grade Count:3 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |