Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.206 J/cm² | 0.980 ft-lb/in² | ASTM D256 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Charpy Impact, Notched | 0.206 J/cm² | 0.980 ft-lb/in² | ASTM D256 |
Plenco 3356 Phenolic, Granular, Compression Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Charpy Impact, Notched | 0.206 J/cm² | 0.980 ft-lb/in² | ASTM D256 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Charpy Impact, Notched | 0.206 J/cm² | 0.980 ft-lb/in² | ASTM D256 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Charpy Impact, Notched | 0.206 J/cm² | 0.980 ft-lb/in² | ASTM D256 |
Plenco 4485 Phenolic, Granular, Transfer Molded PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a.. |