Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 650 MPa @Temperature 23.0 °C |
94300 psi @Temperature 73.4 °F |
prEN2580 Type B |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |