Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0650 MPa @Strain 25.0 % |
9.43 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 446 NDN NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Compressive Yield Strength | 0.0650 MPa @Strain 25.0 % |
9.43 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |