Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 276 MPa @Temperature 25.0 °C |
40000 psi @Temperature 77.0 °F |
Compression After Impact, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 276 MPa @Temperature 71.0 °C |
40000 psi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel |
|||
Compressive Yield Strength | 276 MPa @Temperature 71.0 °C |
40000 psi @Temperature 160 °F |
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel |
|||
Compressive Yield Strength | 276 MPa @Temperature 177 °C |
40000 psi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F161; Fiber: 150-1/2Information provided by HexCel |