Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1181 MPa @Temperature 232 °C |
171300 psi @Temperature 450 °F |
IM7 (12K); [0°]8 |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |