Polymer Property : Compressive Yield Strength = 276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 276 MPa

@Temperature 25.0 °C
40000 psi

@Temperature 77.0 °F
Compression After Impact, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber
Information provided by HexCel
Compressive Yield Strength 276 MPa

@Temperature 71.0 °C
40000 psi

@Temperature 160 °F
1/2 hr
Hexcel® HexPly® F515 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F515; Fiber 75-1/0Information provided by HexCel
Compressive Yield Strength 276 MPa

@Temperature 71.0 °C
40000 psi

@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
Hexcel® HexPly® F522 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F522; Fiber: 75-1/0Information provided by HexCel
Compressive Yield Strength 276 MPa

@Temperature 177 °C
40000 psi

@Temperature 351 °F
Hexcel® F161 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F161; Fiber: 150-1/2Information provided by HexCel