Compressive Yield Strength 1410 MPa

@Temperature 82.0 °C
205000 psi

@Temperature 180 °F
0°, Dry
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber
Information provided by HexCel
Compressive Yield Strength 1410 MPa

@Temperature 149 °C
205000 psi

@Temperature 300 °F
0°, Wet
Hexcel® HexPly® 954-2A Curing Cyanate Resin, IM7 Fiber
Information provided by HexCel