Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 29.0 - 60.0 MPa | 4210 - 8700 psi | Average value: 42.4 MPa Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Ball Indentation Hardness | 36.0 - 60.0 MPa | 5220 - 8700 psi | Average value: 48.6 MPa Grade Count:10 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Ball Indentation Hardness | 54.0 - 60.0 MPa @Time 30.0 sec |
7830 - 8700 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Ball Indentation Hardness | 56.0 - 60.0 MPa | 8120 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 57.0 - 60.0 MPa | 8270 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2 Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 57.0 - 60.0 MPa | 8270 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 817 PTFE, 60% Bronze Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 50.0 - 60.0 MPa | 7250 - 8700 psi | ISO 2032-N132 |
Adamas Adalon® 266 PTFE, Mineral/Glass Bubbles Filler Information provided by Adamas, HPM |