Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 60.0 - 120 MPa | 8700 - 17400 psi | Average value: 82.9 MPa Grade Count:24 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Ball Indentation Hardness | 110 - 120 MPa | 16000 - 17400 psi | Average value: 115 MPa Grade Count:7 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Ball Indentation Hardness | 95.0 - 120 MPa | 13800 - 17400 psi | Average value: 109 MPa Grade Count:7 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Ball Indentation Hardness | 90.0 - 120 MPa | 13100 - 17400 psi | ISO 2032 |
Adamas Lakinor® U PVDF Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 100 - 120 MPa | 14500 - 17400 psi | ISO 2032-N132 |
Adamas Adalon® 463 PTFE, 15% Special Polyimide Information provided by Adamas, HPM |
|||
Ball Indentation Hardness | 80.0 - 120 MPa | 11600 - 17400 psi | Average value: 99.3 MPa Grade Count:26 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Ball Indentation Hardness | 35.0 - 120 MPa | 5080 - 17400 psi | Average value: 88.6 MPa Grade Count:14 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |