Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 64.0 MPa | 9280 psi | DIN 53456 |
Global PP-2540-K Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-paint drum, storage & transport containerInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 64.0 MPa | 9280 psi | DIN 53456 |
Global PP-3342-M Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-housewares, cookwareInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 64.0 MPa | 9280 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |