Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 8700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 60.0 MPa
8700 psi
ISO 2039-1
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Ball Indentation Hardness 60.0 - 120 MPa
8700 - 17400 psi
Average value: 82.9 MPa Grade Count:24
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Ball Indentation Hardness 60.0 MPa
8700 psi
Fm=358N; Ø 50x4mm; ISO 2039-1
SYNTHOS Krasten® 662E High Impact Polystyrene
High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa..
Ball Indentation Hardness 60.0 MPa
8700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® AS LF 20 PA66-Z20
Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert..
Ball Indentation Hardness 60.0 MPa
8700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BS EC PA6
Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro..
Ball Indentation Hardness 60.0 MPa
8700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BS/2 PA6
Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior..
Ball Indentation Hardness 60.0 MPa
8700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4128 black 9221 PA610
Product description: Grilamid XE 4128 black 9221 is a modified high viscosity Polyamide 610 for extrusion as well as injection molding. A characteristic of tubes made out of this material is the hig..
Ball Indentation Hardness 60.0 MPa
8700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BR 40 PA6
Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie..
Ball Indentation Hardness 60.0 - 64.0 MPa
8700 - 9280 psi
ISO 2032-N132
Adamas Adalon® 992 Modified PTFE
Information provided by Adamas, HPM
Ball Indentation Hardness 60.0 - 140 MPa
8700 - 20300 psi
Average value: 100 MPa Grade Count:4
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Ball Indentation Hardness 60.0 MPa
8700 psi
358 N/30s; ISO 2039
Borealis ME268Al Polypropylene Compound, Mineral Filled
ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par..
Ball Indentation Hardness 60.0 - 62.0 MPa
8700 - 8990 psi
ISO 2032
Adamas Adalon® 510 PTFE, 5% MoS2
Information provided by Adamas, HPM
Copyright © lookpolymers.com All Rights Reserved