Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 8270 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 57.0 MPa
8270 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene
Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 57.0 MPa
8270 psi
H385/30; ISO 2039
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled
Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g..
Ball Indentation Hardness 57.0 - 60.0 MPa
8270 - 8700 psi
ISO 2032-N132
Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2
Information provided by Adamas, HPM
Ball Indentation Hardness 57.0 - 60.0 MPa
8270 - 8700 psi
ISO 2032-N132
Adamas Adalon® 817 PTFE, 60% Bronze
Information provided by Adamas, HPM