Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 44.0 MPa | 6380 psi | |
Murtfeldt Original Material ”S”® plus + GB Polyethylene, Glass Bead Filled The balanced quantity of micro glass beads in Material ”S”® plus+ GB provides the combined benefits of extremely high molecular weight polyethylene and glass. The glass beads that protrude from .. |
|||
Ball Indentation Hardness | 44.0 MPa | 6380 psi | ISO 2039 |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Ball Indentation Hardness | 44.0 MPa | 6380 psi | 358 N/30s; ISO 2039 |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Ball Indentation Hardness | 44.0 - 48.0 MPa | 6380 - 6960 psi | ISO 2032-N132 |
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue Information provided by Adamas, HPM |