Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 210 MPa | 30500 psi | ISO 2039-1 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PA6 GF Akulon GF - Dry Polyamide 6 reinforced with the addition of 30% glass fibre and graphite. The glass charge makes the material highly resistant to abrasion, compression and flexing. Akulon GF is particularly suitabl.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30 PA6-GF30 Product description: Grilon BG-30 is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 has the following important properties: High stiffnessGood balance between stre.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30 S FA PA6-GF30 Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy .. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-30/2 PA6-GF30 Product description: Grilon BG-30/2 is a heat stabilized, normal viscosity PA6 injection molding grade with 30% glass fibers. Grilon BG-30/2 has the following important properties: High stiffnessGoo.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 PA666-GF30 Product description: Grilon TSG-30/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30/4 has the following important properties: Good flo.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4063 black 9238 PA6T/66-GF30 Product description: Grivory XE 4063 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 5026 (BG-30 H) PA6-GF30 Product description: Grilon B XE 5026 (BG-30 H) black 9922 is a high heat stabilized, 30% glass fiber reinforced PA6- Injection molding grade with modified flowability. Grilon B XE 5026 (BG-30 H) bl.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | Measured by nanoindentation |
Dow SiLK™ D Semiconductor Dielectric Resin SiLK™ D resin provides a more controlled coefficient of thermal expansion (CTE) profile at elevated temperatures as compared to earlier versions of SiLK™ resin.Information provided by Dow |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation .. |
|||
Ball Indentation Hardness | 210 MPa @Load 36.5 kg |
30500 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Ball Indentation Hardness | 210 MPa @Load 36.5 kg |
30500 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF35 Polyamide 6 - Glass Fiber Reinforced 35% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Ball Indentation Hardness | 210 MPa | 30500 psi | H961/30; ISO 2039-1 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Ball Indentation Hardness | 210 MPa @Load 36.5 kg |
30500 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |