Polymer Property : Ball Indentation Hardness = 150 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 70.0 - 150 MPa
10200 - 21800 psi
ISO.2039-2
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Ball Indentation Hardness 70.0 - 150 MPa
10200 - 21800 psi
ISO.2039-2
Polimersan Plastics POLIPA® (PA 6) Polyamide
POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc..
Ball Indentation Hardness 66.0 - 150 MPa
9570 - 21800 psi
Average value: 138 MPa Grade Count:13
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Ball Indentation Hardness 81.0 - 150 MPa
11700 - 21800 psi
Average value: 140 MPa Grade Count:16
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Ball Indentation Hardness 110 - 150 MPa
16000 - 21800 psi
Average value: 129 MPa Grade Count:9
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Ball Indentation Hardness 110 - 150 MPa
16000 - 21800 psi
ISO 2032
Adamas Adalon® 466 PTFE, Mineral/Organic Filler
Information provided by Adamas, HPM
Ball Indentation Hardness 70.0 - 150 MPa
10200 - 21800 psi
Average value: 112 MPa Grade Count:3
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Ball Indentation Hardness 76.0 - 150 MPa
11000 - 21800 psi
Average value: 125 MPa Grade Count:3
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Ball Indentation Hardness 70.0 - 150 MPa
10200 - 21800 psi
Average value: 109 MPa Grade Count:11
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..