Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 120 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 60.0 - 120 MPa
8700 - 17400 psi
Average value: 82.9 MPa Grade Count:24
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Ball Indentation Hardness 110 - 120 MPa
16000 - 17400 psi
Average value: 115 MPa Grade Count:7
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Ball Indentation Hardness 95.0 - 120 MPa
13800 - 17400 psi
Average value: 109 MPa Grade Count:7
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Ball Indentation Hardness 90.0 - 120 MPa
13100 - 17400 psi
ISO 2032
Adamas Lakinor® U PVDF
Information provided by Adamas, HPM
Ball Indentation Hardness 100 - 120 MPa
14500 - 17400 psi
ISO 2032-N132
Adamas Adalon® 463 PTFE, 15% Special Polyimide
Information provided by Adamas, HPM
Ball Indentation Hardness 80.0 - 120 MPa
11600 - 17400 psi
Average value: 99.3 MPa Grade Count:26
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Ball Indentation Hardness 35.0 - 120 MPa
5080 - 17400 psi
Average value: 88.6 MPa Grade Count:14
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Copyright © lookpolymers.com All Rights Reserved