Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 93.0 MPa | 13500 psi | ISO 2039-1 |
Nilit FRIANYL B63 SI20 Nylon 6 for injection molding Nylon 6 for injection molding, ionomer impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 93.0 MPa | 13500 psi | 132N/10s; ISO 2039 |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Ball Indentation Hardness | 93.0 MPa | 13500 psi | H358/30; ISO 2039-1 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |