Mechanical Properties Metric English Comments
Ball Indentation Hardness 54.0 MPa
7830 psi
DIN 53456
Global PP-3300-RC Polypropylene Random Copolymer
Description-medium stiffness, low melting temperatures, very good for seal Applications-thin-walled parts, audio tapes, cupsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 54.0 - 60.0 MPa

@Time 30.0 sec
7830 - 8700 psi

@Time 0.00833 hour
DIN 53 456
Hippe PE 300 Polyethylene
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall..
Ball Indentation Hardness 54.0 - 56.0 MPa
7830 - 8120 psi
ISO 2032
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 54.0 - 56.0 MPa
7830 - 8120 psi
ISO 2032
Adamas Adalon® 477 PTFE, 20% Aramid Fiber