Category | Polymer , Thermoplastic , Fluoropolymer , PTFE |
Manufacturer | Adamas |
Trade Name | Adalon® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Adamas Adalon® 477 PTFE, 20% Aramid Fiber.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.93 - 1.96 g/cc | 1.93 - 1.96 g/cc | ASTM D792 |
Deformation | 1.7 - 3.0 % | 1.7 - 3.0 % | ASTM D621 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 57 - 59 | 57 - 59 | ASTM D2240 |
Ball Indentation Hardness | 54.0 - 56.0 MPa | 7830 - 8120 psi | ISO 2032 |
Tensile Strength at Break | 16.0 - 18.0 MPa | 2320 - 2610 psi | ASTM D4745-97 |
Elongation at Break | 180 - 195 % | 180 - 195 % | ASTM D4745-97 |
Coefficient of Friction, Static | 0.30 - 0.40 | 0.30 - 0.40 | ASTM D1894 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
Melting Point | 327 °C | 621 °F | DSC |
Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
Flammability, UL94 | V-0 | V-0 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | ASTM D257 |
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |