Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 275 MPa | 39900 psi | H 961/30; ISO 2039/P1 |
Hexion Bakelite™ X22 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Pot handles, operating controls, electrical isolators, housing parts.Informati.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | H 961/30; ISO 2039/P1 |
Hexion Bakelite™ X24 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled.Application areas: Operating controls, housing parts, lamp holders.Information provided by Bak AGBak AG became a part of Hexion in 2005. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | H 961/30; ISO 2039/P1 |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50 Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | ISO 2039-1 |
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data) This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s.. |
|||
Ball Indentation Hardness | 275 MPa | 39900 psi | H 961/30; ISO 2039/P1 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |