Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 270 MPa | 39200 psi | ISO 2039-1 |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 270 - 360 MPa | 39200 - 52200 psi | Average value: 320 MPa Grade Count:11 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30 Grivory TH2V-3H LF is a glass fiber reinforced (30%), PTFE modified engineering thermoplastic based on semi-crystalline partially aromatic copolyamide. Polymer designation acc. ISO: PA6T/66 Polymer .. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HTV-3H1 nat PA6T/6I-GF30 Product description: Grivory HTV-3H1 natural is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA black 9225 is a 30 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: .. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 FWA nat PA6T/6I-GF30 Product description: Grivory HT1V-3 FWA natural is a 30 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Ball Indentation Hardness | 270 MPa @Load 36.5 kg |
39200 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | HB 961/30; ISO 2039-1 |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Ball Indentation Hardness | 270 MPa | 39200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Ball Indentation Hardness | 270 - 290 MPa | 39200 - 42100 psi | Average value: 283 MPa Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |