Polymer Property : Film Tensile Strength at Yield, MD = 2900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 20.0 MPa

@Thickness 0.430 mm,
Temperature 23.0 °C
2900 psi

@Thickness 0.0169 in,
Temperature 73.4 °F
ASTM D638
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required.
Film Tensile Strength at Yield, MD 20.0 MPa

@Thickness 0.250 mm,
Temperature 23.0 °C
2900 psi

@Thickness 0.00984 in,
Temperature 73.4 °F
ASTM D638
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required.
Film Tensile Strength at Yield, MD 20.0 MPa

@Thickness 0.0200 mm
2900 psi

@Thickness 0.000787 in
ISO 527-3
Total MDPE HF 513 Medium Density Polyethylene, Blown Film
MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic..
Film Tensile Strength at Yield, MD 20.0 MPa

@Thickness 0.0400 mm
2900 psi

@Thickness 0.00157 in
ISO 527-3
Total MDPE HT 514 Medium Density Polyethylene, Blown Film
MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic..