Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 59.7 J @Tempering Temp. 204 °C |
44.0 ft-lb @Tempering Temp. 400 °F |
austenitizied at 1550°F then tempered; C-notch |
Crucible Steel CSM® 6 Tool Steel, AISI A6 CSM 6 is an air hardening tool steel offering moderate wear resistance and toughness. It may be hardened from a low hardening temperature for easy heat treatment.Information provided by Crucible Ind.. |