Polymer Property : Flexural Stiffness = 784.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Stiffness 784.5 MPa
113800 psi
Olsen; ASTM D747
Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene
HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3...
Flexural Stiffness 784.5 MPa
113800 psi
Olsen; ASTM D747
Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene
HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplic..