Polymer Property : Gardner Impact = 26.6 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 13.8 - 36.0 J
10.2 - 26.6 ft-lb
Average value: 28.6 J Grade Count:10
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
Gardner Impact 22.0 - 36.0 J

@Temperature -30.0 - -30.0 °C
16.2 - 26.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 33.7 J Grade Count:15
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
Gardner Impact 34.0 - 36.0 J

@Temperature -30.0 - -30.0 °C
25.1 - 26.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 36.2 J Grade Count:6
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m..
Gardner Impact 34.0 - 36.0 J
25.1 - 26.6 ft-lb
Average value: 34.5 J Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Gardner Impact 2.26 - 36.0 J
1.67 - 26.6 ft-lb
Average value: 29.1 J Grade Count:52
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Gardner Impact 1.00 - 36.0 J

@Temperature -30.0 - -20.0 °C
0.738 - 26.6 ft-lb

@Temperature -22.0 - -4.00 °F
Average value: 19.8 J Grade Count:41
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..