Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 11.8 J | 8.70 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT NN-40LCF/001 Grey Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 11.8 J | 8.70 ft-lb | ASTM D5420 |
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Gardner Impact | 11.8 J | 8.70 ft-lb | ASTM D5420 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Gardner Impact | 11.8 J | 8.70 ft-lb | ASTM D5420 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |