Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 27.1 J @Temperature -18.0 °C |
>= 20.0 ft-lb @Temperature -0.400 °F |
Gardner |
Network Polymers NPP 25-0110 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 27.1 J @Temperature -18.0 °C |
>= 20.0 ft-lb @Temperature -0.400 °F |
Gardner |
Network Polymers NPP 25-0212 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 27.1 J @Temperature -18.0 °C |
>= 20.0 ft-lb @Temperature -0.400 °F |
Gardner |
Network Polymers NPP 25-2010 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Gardner Impact | 27.1 J | 20.0 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Gardner Impact | 27.1 - 37.0 J | 20.0 - 27.3 ft-lb | Average value: 35.5 J Grade Count:11 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Gardner Impact | 27.1 J | 20.0 ft-lb | 0.125 in; ASTM D3029 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Gardner Impact | 27.1 J @Temperature -30.0 °C |
20.0 ft-lb @Temperature -22.0 °F |
ASTM D3029, tested in accordance with ASTM D5420 |
LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer Description: Pro-faxâ„¢ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of.. |
|||
Gardner Impact | 27.1 J @Temperature 22.8 °C |
20.0 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |