Polymer Property : Gardner Impact = 14.58 ft-lb
Polymer Property :
Gardner Impact =
14.58 ft-lb
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Gardner Impact
19.77
J
14.58
ft-lb
ASTM D3029
Multibase Nylex™ 2185 HF Black Polyamide + PP
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase