Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.70 J | 1.99 ft-lb | ASTM D5420 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Gardner Impact | 2.70 J | 1.99 ft-lb | ASTM D5420 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Gardner Impact | 2.70 J | 1.99 ft-lb | ASTM D3029 |
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |