Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D5420 |
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D5420 |
RheTech Products M25P251-01A 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsInternal I/P componentsFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D5420 |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D3029 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D3029 |
Polymer Resources PEI-GP1-TFE5 Polyetherimide, 5% PTFE, Flame Retardant Polyetherimide, General Purpose, 5% PTFE, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 2.26 J | 1.67 ft-lb | ASTM D5420 |
RheTech Products M25P251-01 25% Mica Reinforced Polypropylene Copolymer, Black Applications: Fan shroudsGlove box binFiller panelsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D5420 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 J @Temperature -28.9 °C |
1.67 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Gardner Impact | 2.26 - 36.0 J | 1.67 - 26.6 ft-lb | Average value: 29.1 J Grade Count:52 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |