Mechanical Properties Metric English Comments
Gardner Impact 2.03 J
1.50 ft-lb
ASTM D5420
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural
Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 2.03 J
1.50 ft-lb
ASTM D5420
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 2.03 J
1.50 ft-lb
ASTM D5420
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural
Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Gardner Impact 2.03 J

@Temperature -28.9 °C
1.50 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene
DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved