Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.80 J | 1.33 ft-lb | ASTM D5420 |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.80 J | 1.33 ft-lb | ASTM D5420 |
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.80 J | 1.33 ft-lb | ASTM D5420 |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.80 J | 1.33 ft-lb | ASTM D5420 |
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 30% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 40% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Homopolymer Polypropylene 50% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 11 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Polypropylene Copolymer 30% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Gardner Impact | 1.80 J | 1.33 ft-lb | ASTM D5420-93 |
Multibase Multi-ABS 3525 Black Moisture content is 0.08%.Data provided by Multibase. |
|||
Gardner Impact | 1.81 J @Temperature 23.0 °C |
1.33 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 15 MFI Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Gardner Impact | 1.80 - 22.6 J | 1.33 - 16.7 ft-lb | Average value: 16.7 J Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |