Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-01UV 20% Talc Reinforced Polypropylene, UV Stabilized, General Purpose Black Applications: Durable goodsElectronics housingsIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-248 20% Talc Reinforced Polypropylene, General Purpose Grey Applications: Durable goodsElectronics housingsHVAC ducts - air distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P100-517UV 20% Talc Reinforced Polypropylene, UV Stabilized, Interior DX9 Black Applications: Center consolesIP componentsClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products HP525-01 30% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Center consolesInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.13 J | 0.830 ft-lb | ASTM D5420 |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |