Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 9.717 J | 7.167 ft-lb | ASTM D3029 |
Multibase Nylex™ 2185 R15 Polyamide + PP Glass fiber reinforcement, 15% Filler by Weight. Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Metho.. |