Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.03 J | 1.50 ft-lb | ASTM D5420 |
RheTech Products GC10P250-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.03 J | 1.50 ft-lb | ASTM D5420 |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.03 J | 1.50 ft-lb | ASTM D5420 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Gardner Impact | 2.03 J @Temperature -28.9 °C |
1.50 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |