Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 154 kJ/m² @Temperature 23.0 °C |
73.3 ft-lb/in² @Temperature 73.4 °F |
DAM; Short specimen; ASTM D1822 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612