Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 147 J/cm | 0.275 ft-lb/mil | H.25 Tup, Method A; ASTM D-4226 |
Axiall 5055 Rigid PVC, Extrusion, White Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor.. |
|||
Dart Drop Total Energy | 147 J/cm | 0.275 ft-lb/mil | H.25 Tup, Method A; ASTM D-4226 |
Axiall 5055 Rigid PVC, Extrusion, Natural Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p.. |