Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 147 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.276 ft-lb/mil @Thickness 0.125 in, Temperature 73.0 °F |
Procedure A, 0.125" Conical Dart |
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Dart Drop Total Energy | 147 J/cm | 0.275 ft-lb/mil | H.25 Tup, Method A; ASTM D-4226 |
Axiall 5055 Rigid PVC, Extrusion, White Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor.. |
|||
Dart Drop Total Energy | 147 J/cm | 0.275 ft-lb/mil | H.25 Tup, Method A; ASTM D-4226 |
Axiall 5055 Rigid PVC, Extrusion, Natural Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p.. |