Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 33.8 MPa

@Temperature 20.0 °C
4900 psi

@Temperature 68.0 °F
DuPont™ Tedlar® SP TTR5JSH9 Clear Polyvinyl Fluoride Film
Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning ex..