DuPont™ Tedlar® SP TTR5JSH9 Clear Polyvinyl Fluoride Film

Category Polymer , Film , Thermoplastic , Fluoropolymer
Manufacturer DuPont
Trade Name Tedlar® SP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Tedlar® SP TTR5JSH9 Clear Polyvinyl Fluoride Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning expected of PVF film. Tedlar® SP also offers custom color capability not previously available in PVF film. Tedlar® SP is an unoriented film. It possesses high elongation and moderate yield stress. After lamination using conventional means, it can be easily embossed and will maintain high pattern definition. Tedlar® SP can also be subjected to high levels of forming without significant recovery stresses.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 155 %

@Temperature 20.0 °C
155 %

@Temperature 68.0 °F
250 %

@Temperature 50.0 °C
250 %

@Temperature 122 °F
260 %

@Temperature 100 °C
260 %

@Temperature 212 °F
280 %

@Temperature 75.0 °C
280 %

@Temperature 167 °F
Film Elongation at Break, TD 150 %

@Temperature 20.0 °C
150 %

@Temperature 68.0 °F
220 %

@Temperature 50.0 °C
220 %

@Temperature 122 °F
255 %

@Temperature 75.0 °C
255 %

@Temperature 167 °F
275 %

@Temperature 100 °C
275 %

@Temperature 212 °F
Film Tensile Strength at Break, MD 10.3 MPa

@Temperature 100 °C
1500 psi

@Temperature 212 °F
15.9 MPa

@Temperature 75.0 °C
2300 psi

@Temperature 167 °F
22.1 MPa

@Temperature 50.0 °C
3200 psi

@Temperature 122 °F
33.8 MPa

@Temperature 20.0 °C
4900 psi

@Temperature 68.0 °F
Film Tensile Strength at Break, TD 10.3 MPa

@Temperature 100 °C
1500 psi

@Temperature 212 °F
17.9 MPa

@Temperature 75.0 °C
2600 psi

@Temperature 167 °F
24.8 MPa

@Temperature 50.0 °C
3600 psi

@Temperature 122 °F
33.8 MPa

@Temperature 20.0 °C
4900 psi

@Temperature 68.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified