Polymer Property : Film Tensile Strength at Break, MD = 3200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 22.1 MPa

@Temperature 50.0 °C
3200 psi

@Temperature 122 °F
DuPont™ Tedlar® SP TTR5JSH9 Clear Polyvinyl Fluoride Film
Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning ex..
Film Tensile Strength at Break, MD 22.1 MPa

@Temperature 75.0 °C
3200 psi

@Temperature 167 °F
DuPont™ Tedlar® SP TTRJ10SH9 Clear Polyvinyl Fluoride Film
Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning ex..
Copyright © lookpolymers.com All Rights Reserved