Puncture Energy 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BD310MO Polypropylene Copolymer
BD310MO is a heterophasic copolymer. This grade is characterized by an optimum combination of good impact strength and very high stiffness. This grade is mildly nucleated to maximize the mechanical..
Puncture Energy 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BF330MO Polypropylene Copolymer
BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i..
Puncture Energy 10.0 J

@Temperature 0.000 °C
7.38 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BH980MO Polypropylene Copolymer
BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist..
Puncture Energy 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BH980MO Polypropylene Copolymer
BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist..
Puncture Energy 10.0 J

@Temperature 0.000 °C
7.38 ft-lb

@Temperature 32.0 °F
ISO 6603-2
Borealis BJ356MO Polypropylene Copolymer
BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle..
Puncture Energy 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BJ356MO Polypropylene Copolymer
BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle..
Puncture Energy 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
ISO 6603-2
Borealis BJ380MO Polypropylene Copolymer